1992 Start of production with gradient TiN, CrN, and TiCN coatings and tool polishing
1994 TiCN multilayers
1998 Start of production for WS2 lubricant coatings
1998 - 2000 Process and subprocess optimisation following a integrated project with the Berlin Technology Foundation (Technologiestiftung Berlin) and the Technical University Berlin (TU Berlin)
2000 Start of production for TiAlN coatings
2002 Expansion of existing installations by 400 mm and start of coatings for parts up to 1000 mm
2006 Setup of a fully CNC PVD system for depositing user-defined multilayer-coatings and coatinglayer variations